Detail produk:
|
| Bahan: | Anisotropic Bonded Samarium Iron Nitrogen Magnet | Aplikasi: | Magnet Industri, Motor, Otomotif, Disesuaikan |
|---|---|---|---|
| Nilai: | MGT-IS-230,MGT-IS-240,MGT-IS-250,MGT-IS-260 | Ukuran: | 1mm-100mm, Disesuaikan |
| Arah Magetik: | Aksial, Radial, Malaikat Miring Magnet, Disesuaikan | Lingkungan: | RoHs, Jangkauan, SGS, MSDS |
| Lapisan: | Tidak dilapisi, Disesuaikan | Warna: | Hitam atau Coklat Hitam |
| Cahaya Tinggi: | Magnet Nitrogen Besi Samarium,Magnet Nitrogen Besi Berikat Anisotropik,Magnet Pompa Air SmFeN Injeksi |
||
Anisotropic Bonded Samarium Besi Nitrogen Magnet Injeksi SmFeN Magnet Pompa Air Magnet
Aplikasi
Fitur
| Senyawa Anisotropic SmFeN+Ferrite(PA12) untuk Injeksi | ||||||||||
| HCSFY230L | HCSFY240L | HCSFY250L | HCSFY260L | HCSFY270L | HCSY280L | HCSY290L | ||||
| 单位 Satuan | SY+TA | SY+TA | SY+TA | SY+TA | SY+TA | SY | SY | |||
| Properti Magnetik | Induksi Residu | Sdr | mT | 330-370 | 400-490 | 500-540 | 540-580 | 590-630 | 500-600 | 570-680 |
| kg | 3.3-3.7 | 4.0-4.9 | 5.0-5.4 | 5.4-5.8 | 5.9-6.3 | 5.0-6.0 | 5.7-6.8 | |||
| Kekuatan Koersif | Hcb | kA/m | 159-191 | 183-263 | 247-279 | 289-318 | 289-318 | 240-320 | 279-359 | |
| kOe | 2.0-2.4 | 2.3-3.3 | 3.1-3.5 | 3.6-4.0 | 3.6-4.0 | 3.0-4.0 | 3,5-4,5 | |||
| Koersivitas Intrinsik | Hcj | kA/m | 223-303 | 350-517 | 398-438 | 430-462 | 438-494 | 240-560 | 340-640 | |
| kOe | 2.8-3.8 | 4.4-6.5 | 5.0-5.5 | 5.4-5.8 | 5.5-6.2 | 3.0-7.0 | 4.0-8.0 | |||
| Max.Produk Energi | (BH)maks | kJ/cm3 | 20-28 | 30-40 | 40-44 | 48-52 | 56-64 | 60-68 | 68-76 | |
| MGOe | 2.5-3.5 | 4.0-5.0 | 5.0-5.5 | 6.0-6.5 | 7.0-8.0 | 7.5-8.5 | 8.5-9.5 | |||
| Properti fisik | Kepadatan | ρ | g/cm3 | 3.5-3.9 | 3.6-4.0 | 3.8-4.2 | 4.0-4.3 | 4.1-4.4 | 3.8-4.3 | 4.0-4.5 |
| Laju Aliran Leleh | MFR | g/10 mnt | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | |
| (270℃ 10kg) | ||||||||||
| Penyusutan | % | 0,6-1 | 0,6-1 | 0,6-1 | 0,6-1 | 0,6-1 | 0,6-1 | 0,6-1 | ||
| Kekuatan Tarik | ASTM-D638 | MPa | 45 | 46 | 47 | 48 | 49 | 45 | 45 | |
| Modulus lentur | ASTM-D790 | MPa | 75 | 78 | 80 | 85 | 86 | 75 | 75 | |
| Modulus lentur | ASTM-D790 | IPK | 15 | 16 | 16 | 17 | 17 | 15 | 15 | |
| Kekuatan Dampak IZOD | ASTM-D256 | (kJ/m2) | 7.8 | 8.2 | 8.4 | 8.1 | 8.1 | 7.8 | 7.8 | |
| Proses Pencetakan Injeksi | ||||||||||
| Cincin LT-35T (35ton). Φ10xΦ7x10 |
Pra-pengeringan | ℃/jam | 80/4 | |||||||
| Temp barel. | T1 | ℃ | 230 | 230 | 230 | 230 | 230 | 210 | 210 | |
| T2 | ℃ | 245 | 245 | 245 | 245 | 245 | 230 | 230 | ||
| T3 | ℃ | 250 | 250 | 250 | 250 | 250 | 235 | 235 | ||
| Suhu cetakan | ℃ | 80 | 80 | 80 | 80 | 80 | 80 | 80 | ||
| Tekanan | MPa (kg/cm2) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
117.5 (1199) |
117.5 (1199) |
||
| Kecepatan | % | 60 | 60 | 60 | 60 | 60 | 60 | 60 | ||
| 1. Kondisi cetakan untuk referensi pelanggan, suhu tertinggi laras injeksi nilon tidak boleh melebihi 260 derajat. | ||||||||||
| 2. Dapat disesuaikan sesuai dengan kebutuhan pelanggan | ||||||||||
![]()
![]()